Both 2024-T4 aluminum and 2117 aluminum are aluminum alloys. Both are furnished in the T4 temper. They have a very high 98% of their average alloy ...
People also ask
Both 2024-T3 aluminum and 2117 aluminum are aluminum alloys. They have a very high 98% of their average alloy composition in common.
Apr 2, 2021 · The 2117 is “structural” quality aluminum alloyed for making rivits. 5056 is soft, used in forming and punching. I would stick with 2117 ...
Jul 8, 2009 · The 2020 is 13.5 gpi, and the 2117 is 12.0. The 2020 has a deflection of .426 and a spine rating of 77#. The 2117 has a deflection of .400 ...
Jul 27, 2010 · If you are still shooting 60 lbs the 2117-2216-2315 all all good choices for that draw length. If you shorten the length of the arrow up you can ...
This is an age hardenable alloy of aluminum and copper. Corrosion resistance is fair. However the forming and strength characteristics are good. Applications ...
Alloy 2017-T4 exhibited relatively high strength and high ductility in the naturally aged condition. Tensile elongation was ~22% at a yield strength of 280 MPa ...
Sep 15, 2004 · I have been heat treating, driving, and testing 2017 "D" rivets and 2117 "AD" rivets and have been getting shear strengths about 15% less ...
... 2117, 2017,2024, and 5056 are considered standard. ALLOY 1100 RIVETS.—Alloy 1100 rivets are supplied as fabricated (F) temper, and are driven in this condition.
Jan 29, 2004 · The 2314 is * shade bit stiffer, but not enough to really worry about. Also it is slightly lighter than the 2117 so it should shoot * bit ...